08/06/2026
Bad material, bad peel test. Don't risk your pipeline projects!
A weak joint can ruin an entire multi-million dollar water or gas project. See how ERA ensures zero-leakage safety through rigorous testing.
Inside the ERA Lab: Electrofusion Peel Testing
Specimen preparation according to standard sizes.
Securely clamped in the tensile testing machine.
Constant speed tension applied until final peeling.
The Ultimate Proof: The pipe tore apart, but the welding zone remained flawlessly intact!
ERA Advantages:
100% Virgin PE100 Raw Material
Certified by CE, KITEMARK, WATERMARK
Joint strength exceeds the pipe itself
Partner with ERA for worry-free installations.
Drop a comment below or Message us directly to discuss bulk pricing and cooperation!